PostPosted: Sat Jul 18, 2020 12:41 pm 
Offline
Contributing Member
Contributing Member

Joined: Tue Dec 17, 2013 10:52 pm
Posts: 3072
First name: Don
Last Name: Parker
City: Charleston
State: West Virginia
Zip/Postal Code: 25314
Country: USA
Focus: Build
Status: Amateur
I am applying Enduro Var with a foam brush, and waiting a little less than an hour between coats; no sanding in between. I put a single coat on a few days ago, then sanded with 320 to eliminate drips and scuff it up, and now I have put on two coats so far today. I was planning on putting one more coat on at least, but I can just keep going and put more coats on, leaving less than an hour between, if there is no downside to doing so. Or, I can stop at 3 coats for today, sand it tomorrow, and put on another 3 coats. And then I can get back to it a few days later (sanding before applying another 2-3 coats).

Thoughts? I don't want to overdo the coats if more than 3 in a day is too much, but I also don't want to waste the time I have available.

Thanks for any wisdom.


Top
 Profile  
 
PostPosted: Sat Jul 18, 2020 12:52 pm 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Mon Apr 16, 2012 12:47 pm
Posts: 2522
First name: Jay
Last Name: De Rocher
City: Bothell
State: Washington
I used EnduroVar for the first time on my last instrument and brushed it on. I did 8 coats 1 hour apart on the first day, level sanded the next morning, and then did 6 coats 1 hour apart that day. It worked great. Temperature at the time was 70 degrees.

The schedule I used was based on Woodie G's schedule for brushing on EnduroVar.

_________________
Once in a while you get shown the light in the strangest of places if you look at it right - Robert Hunter


Top
 Profile  
 
PostPosted: Sat Jul 18, 2020 12:55 pm 
Offline
Contributing Member
Contributing Member

Joined: Tue Dec 17, 2013 10:52 pm
Posts: 3072
First name: Don
Last Name: Parker
City: Charleston
State: West Virginia
Zip/Postal Code: 25314
Country: USA
Focus: Build
Status: Amateur
Perfect info, Jay! I’m following the same brushing instructions; I just wasn’t sure if there was a limit to how much I should try to build in a single day. I’m just going to keep going for a while! I appreciate it.


Top
 Profile  
 
PostPosted: Sat Jul 18, 2020 1:34 pm 
Offline
Koa
Koa
User avatar

Joined: Sun Jun 22, 2014 1:45 pm
Posts: 1483
First name: Michael
Last Name: Colbert
City: Anacortes
State: WA
Focus: Build
J De Rocher wrote:
I used EnduroVar for the first time on my last instrument and brushed it on. I did 8 coats 1 hour apart on the first day, level sanded the next morning, and then did 6 coats 1 hour apart that day. It worked great. Temperature at the time was 70 degrees.

The schedule I used was based on Woodie G's schedule for brushing on EnduroVar.


Do you know how many wet mils each coat is?

Thanks, M


Top
 Profile  
 
PostPosted: Sat Jul 18, 2020 1:42 pm 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Mon Apr 16, 2012 12:47 pm
Posts: 2522
First name: Jay
Last Name: De Rocher
City: Bothell
State: Washington
A brushed-on coat wetted the 2 mil tooth, but not the 3 mil tooth on the gauge so at least 2 mils but less than 3 mils.

_________________
Once in a while you get shown the light in the strangest of places if you look at it right - Robert Hunter



These users thanked the author J De Rocher for the post: Michaeldc (Sat Jul 18, 2020 1:52 pm)
Top
 Profile  
 
PostPosted: Sat Jul 18, 2020 2:21 pm 
Offline
Contributing Member
Contributing Member

Joined: Fri Jan 11, 2013 2:26 pm
Posts: 487
First name: Carl
Last Name: Dickinson
City: Forest Ranch
State: California
Zip/Postal Code: 95942
Country: USA
Focus: Build
Status: Amateur
Here's a finishing schedule I used with modifications on the upright bass. https://generalfinishes.com/blog/2016/0 ... lyurethane


Top
 Profile  
 
PostPosted: Sat Jul 18, 2020 4:05 pm 
Offline
Koa
Koa

Joined: Sat Mar 09, 2019 4:50 pm
Posts: 1256
Location: Goodrich, MI
First name: Ken
Last Name: Nagy
City: Goodrich
State: MI
Focus: Build
Status: Amateur
J De Rocher wrote:
A brushed-on coat wetted the 2 mil tooth, but not the 3 mil tooth on the gauge so at least 2 mils but less than 3 mils.



I have never heard of a gauge to measure the thickness of a coat of varnish. Who knew? Not me.

_________________
Why be normal?


Top
 Profile  
 
PostPosted: Sat Jul 18, 2020 4:15 pm 
Offline
Koa
Koa
User avatar

Joined: Sun Jun 22, 2014 1:45 pm
Posts: 1483
First name: Michael
Last Name: Colbert
City: Anacortes
State: WA
Focus: Build
Ken Nagy wrote:
J De Rocher wrote:
A brushed-on coat wetted the 2 mil tooth, but not the 3 mil tooth on the gauge so at least 2 mils but less than 3 mils.



I have never heard of a gauge to measure the thickness of a coat of varnish. Who knew? Not me.


Quick google search,

https://www.tooldiscounter.com/product/ ... gIC8vD_BwE

M


Top
 Profile  
 
Display posts from previous:  Sort by  
Post new topic Reply to topic  [ 8 posts ] 

All times are UTC - 5 hours


Who is online

Users browsing this forum: No registered users and 73 guests


You cannot post new topics in this forum
You cannot reply to topics in this forum
You cannot edit your posts in this forum
You cannot delete your posts in this forum
You cannot post attachments in this forum

Jump to:  
Powered by phpBB® Forum Software © phpBB Group
phpBB customization services by 2by2host.com