PostPosted: Sat Jan 13, 2018 5:00 pm 
Offline
Koa
Koa

Joined: Fri Feb 24, 2017 8:43 am
Posts: 1707
Hi guys. As plenty of you know I’m a new builder with way more questions than is good for me. At this point I am working on #5 with wood in the “shop” for 6 and 7.

At this point I have tried several different finish applications and materials, and honestly not done any of them enough to get good at them. I don’t think I’ve found that: “this is my path thing”. However, I find myself consistently leaning toward a spray system finish, although the last was a FP with RL.

That said I’ve yet to GET a spray stem OR pick a finish. I have done one with nitro rattle cans, but honestly the stuff scares the crap out of me for health reasons. I don’t want my kids or wife anywhere near it either. Therefore I’m leaning toward picking a route which involves HVLP and a WB finish.

My process for learning so many different things, at least till now has been: “pick one and go until you get it”. (I mean this is even the 5th OM guitar style haha). So I’m predicting this will me my next attempt when it comes time to finish one out.

So my inquiry comes down to WB finishes I suppose.

In moving away from nitro does one loose a great deal of forgiveness?

Do WB finishes melt into the last layer like nitro or is that due to the chemical solvent, which would be missing.(which I assume is the case)

I apologize for trolling so many questions all the time. I know really mastering something comes down to lots of trial and error, but I’d like to avoid obvious pitfalls that others have made, thus the questions.

Peace
B







Sent from my iPhone using Tapatalk Pro


Top
 Profile  
 
PostPosted: Sat Jan 13, 2018 10:11 pm 
Offline
Brazilian Rosewood
Brazilian Rosewood
User avatar

Joined: Wed Feb 20, 2008 9:12 pm
Posts: 6983
First name: Mike
Last Name: O'Melia
City: Huntsville
State: Alabama
Focus: Build
Status: Semi-pro
Most waterborn finishes have limited melt in. Once you start, you need to keep going. It’s just the nature of the product. Nitro has essentially an unlimited burn in time. You can go days between applications. In my opinion, General Finishes Enduro-Var is one of the best waterborn because of the amber tint. Em 6000 is good because of relative burn in time. But is problematic on dark woods (blue haze). I’ve given up on the waterbornes. Too much risk. Nitro is my favorite. Dangerous? Yes.


Top
 Profile  
 
PostPosted: Sat Jan 13, 2018 11:30 pm 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Mon Apr 16, 2012 12:47 pm
Posts: 2524
First name: Jay
Last Name: De Rocher
City: Bothell
State: Washington
I've only used waterborne finish (EM6000) so I can't tell you about nitro, but I can share my experience with EM6000.

I initially chose to try waterborne because I didn't want to deal with the nasty toxic solvents in nitro, the fire hazard, the need for spark-proof switches, the need to exhaust fumes out of the building, and the off gassing period, etc. I also chose to go with the brush on approach because I don't need a spray apparatus or a spray booth, and I don't have to wear a respirator.

My guitars have been looked over by quite a few builders and many of them assumed the finish was nitro based on its appearance. Many were doubly surprised when I told them it was brushed on. It is definitely possible to get good results. If you are willing and able to set up for spraying, I think that would reduce the total length of time needed to build up the finish compared to the brush on approach.

I have not experienced the "blue haze" problem with EM6000 on dark woods like rosewood, Maccassar ebony, or ziricote. IMO, the rap on EM6000 causing a blue haze is due to applications that were too heavy and/or intervals between applications that were too short.

I've had a few "opportunities" to repair chips in the finish along the edge of the fretboard that I caused when filing the fret ends flush. On both guitars where that happened, the finish had already cured for at least four weeks. The new finish blended in perfectly with the existing finish and the repairs were completely invisible.

Mike is right that you shouldn't stop in the middle of a series of finish applications and start right back up days later like you can with nitro, but if you do a light scuff sanding first, you're good to continue.

I have a pretty detailed protocol written up for how I use EM6000 with notes that I can send you if you are interested. It would give you some info that might help in your process of deciding which way to go.

_________________
Once in a while you get shown the light in the strangest of places if you look at it right - Robert Hunter


Top
 Profile  
 
PostPosted: Sun Jan 14, 2018 9:19 am 
Offline
Brazilian Rosewood
Brazilian Rosewood
User avatar

Joined: Wed Feb 20, 2008 9:12 pm
Posts: 6983
First name: Mike
Last Name: O'Melia
City: Huntsville
State: Alabama
Focus: Build
Status: Semi-pro
I think, between Enduro-Var and EM 6000, the latter is more friendly. You have more time for late coat additions. Guess it crosslinks slower. If I were a new user, I'd go with EM 6000. You can always overspray these at a later date. The issue you will run into is something called "witness lines". That is where you sand through a layer that is not truly melted. If I were going to do something like that, I would sand down a bit, then apply enough coats to avoid that. But, once into that procedure, you never know.

Jay, I am impressed you can brush on with great coats. What exactly is your time between coats (I always used 30 minutes)


Top
 Profile  
 
PostPosted: Sun Jan 14, 2018 10:35 am 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Mon Aug 23, 2010 11:42 pm
Posts: 1703
First name: John
Last Name: Parchem
City: Seattle
State: Wa
Zip/Postal Code: 98177
Country: USA
Focus: Build
Status: Amateur
I have used EM6000 and EM9000. Of the two I would pick EM6000. I have found with both products that the wet film thickness is very important to avoid a blue haze. Em6000 is more forgiving of the two in avoiding a finish with a blue tint. I have had real good results with EM6000. As mentioned by others it is pretty forgiving. Each coat does melt into the previous coat. Em9000 I believe is a lot like EM6000 with a higher amount of solids. I found it very easy to overspray each coat and wind up with a blue instrument. I believe that Jay Litchy uses EM6000 (at least I have seen a video with him using it). I have been very impressed with his finish work.

_________________
http://www.Harvestmoonguitars.com



These users thanked the author johnparchem for the post: Michaeldc (Sun Jan 14, 2018 11:31 am)
Top
 Profile  
 
PostPosted: Sun Jan 14, 2018 10:54 am 
Offline
Koa
Koa
User avatar

Joined: Thu Jan 10, 2008 5:08 am
Posts: 1906
Location: Raleigh, NC
First name: Steve
Last Name: Sollod
Focus: Build
Status: Amateur
+1 for EM6000


You do not have the required permissions to view the files attached to this post.

_________________
Steve Sollod (pronounced sorta like "Solid")
www.swiftcreekguitars.com



These users thanked the author sdsollod for the post: Michaeldc (Sun Jan 14, 2018 11:30 am)
Top
 Profile  
 
PostPosted: Sun Jan 14, 2018 11:30 am 
Offline
Koa
Koa
User avatar

Joined: Sun Jun 22, 2014 1:45 pm
Posts: 1484
First name: Michael
Last Name: Colbert
City: Anacortes
State: WA
Focus: Build
I use EM6000 over Silvertip like Jay Lichty. I shoot 2-3 wet mills per coat, 1hr apart, @ 70° and 43° RH.

I do have a couple of blue guitars out there. Live and learn..

Cheers


Top
 Profile  
 
PostPosted: Sun Jan 14, 2018 1:09 pm 
Offline
Brazilian Rosewood
Brazilian Rosewood

Joined: Wed Feb 20, 2008 7:15 pm
Posts: 7381
First name: Ed
Last Name: Bond
City: Vancouver
Country: Canada
Focus: Build
Status: Professional
Whatever route you go, don't go thinking that WB finishes are non toxic just because the solvents aren't oil based. All the same safety protocols required for nitro also translate to WB, save for explosion proof fans and switches.



These users thanked the author meddlingfool for the post: Michaeldc (Sun Jan 14, 2018 1:12 pm)
Top
 Profile  
 
PostPosted: Sun Jan 14, 2018 3:38 pm 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Mon Apr 16, 2012 12:47 pm
Posts: 2524
First name: Jay
Last Name: De Rocher
City: Bothell
State: Washington
Mike OMelia wrote:
Jay, I am impressed you can brush on with great coats. What exactly is your time between coats (I always used 30 minutes)


I go three hours between coats to err on the side of each coat being dry before the next coat. Since brushing requires adding retarder to keep the EM6000 from setting up as you are brushing it on, I've been conservative about the interval times. To me, this is the one disadvantage of applying with a brush because those intervals add up. I really should do some testing to see how much I can shorten those times and speed up the finishing process overall.

_________________
Once in a while you get shown the light in the strangest of places if you look at it right - Robert Hunter


Top
 Profile  
 
PostPosted: Sun Jan 14, 2018 4:58 pm 
Offline
Brazilian Rosewood
Brazilian Rosewood
User avatar

Joined: Wed Feb 20, 2008 9:12 pm
Posts: 6983
First name: Mike
Last Name: O'Melia
City: Huntsville
State: Alabama
Focus: Build
Status: Semi-pro
Just so you know, I still use EM 6000 and Enduro Var. Just ordered some EM 6000. I just don't feel like its necessary to devote ones self to just one. I used to only do EM 6000. No more. Depends on the guitar. I will take to heart a longer time between coats. I never heard that before.


Top
 Profile  
 
PostPosted: Sun Jan 14, 2018 6:04 pm 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Mon Apr 16, 2012 12:47 pm
Posts: 2524
First name: Jay
Last Name: De Rocher
City: Bothell
State: Washington
I started out originally with four-hour intervals based on what I read several years ago on the Guitar Refinishing and Restoration Forum from EM6000 users using the brush-on method. I don't know if that four hour interval was based on anything like actual testing or not. I reduced that to three hours without problems so it may be possible to go shorter depending on things like temperature, humidity, and thinness of coats.

_________________
Once in a while you get shown the light in the strangest of places if you look at it right - Robert Hunter


Top
 Profile  
 
PostPosted: Mon Jan 15, 2018 11:04 pm 
Offline
Koa
Koa

Joined: Fri Feb 24, 2017 8:43 am
Posts: 1707
meddlingfool wrote:
Whatever route you go, don't go thinking that WB finishes are non toxic just because the solvents aren't oil based. All the same safety protocols required for nitro also translate to WB, save for explosion proof fans and switches.

Of course. Big for me is the fact my family lives where I build (well not in the same room but you get it). If I can avoid super toxicity then ....
But yes ... precautions followed . I agree



Sent from my iPhone using Tapatalk Pro


Top
 Profile  
 
PostPosted: Tue Jan 16, 2018 12:06 am 
Offline
Brazilian Rosewood
Brazilian Rosewood
User avatar

Joined: Wed Feb 20, 2008 9:12 pm
Posts: 6983
First name: Mike
Last Name: O'Melia
City: Huntsville
State: Alabama
Focus: Build
Status: Semi-pro
The waterborne finishes we are talking about are not super toxic. Even nitro is not super toxic (but it ain’t super nice). Now, the modern stuff they paint cars and airplanes with, totally different subject. Same with poly’s for guitars. Nonetheless less, if it ain’t pure air, use a mask. A good one.


Top
 Profile  
 
PostPosted: Tue Jan 16, 2018 9:48 am 
Offline
Koa
Koa

Joined: Mon Jul 11, 2005 5:17 am
Posts: 1011
Location: United States
City: Tyler
State: Texas
Most of the MSDS I have read have waterbourne having the same levels of concern as nitro with the exception of flammability. You should wear a mask and protect skin with both.


Top
 Profile  
 
PostPosted: Tue Jan 16, 2018 11:38 am 
Offline
Brazilian Rosewood
Brazilian Rosewood

Joined: Fri Dec 14, 2007 3:21 pm
Posts: 3395
Location: Alexandria MN
Are your necks holding up with the waterbased? Breaking down where the arm hangs over the lower bout? Those were some of my issues. Do they dull over time, another issue I saw.

I used KTM9 and EM6000 years back, (Never Enduro-Var) both brush and spray. Was encouraged by the likes of John Greven, Mike Doolin, and Gerald Shepard. Even Charles Fox. I was never able to achieve a finish that looked as good or held up as well as a professional nitro or catalyzed urethane application. I don't know about Greven but I think the others abandoned waterbased.

Has anyone here been selling guitars in the 3K plus range over a long period of time and finding customers satisfied with a waterbased finish?

_________________
It's not what you don't know that hurts you, it's what you do know that's wrong.


Top
 Profile  
 
PostPosted: Tue Jan 16, 2018 12:42 pm 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Mon Aug 23, 2010 11:42 pm
Posts: 1703
First name: John
Last Name: Parchem
City: Seattle
State: Wa
Zip/Postal Code: 98177
Country: USA
Focus: Build
Status: Amateur
Terence Kennedy wrote:
Are your necks holding up with the waterbased? Breaking down where the arm hangs over the lower bout? Those were some of my issues. Do they dull over time, another issue I saw.

I used KTM9 and EM6000 years back, (Never Enduro-Var) both brush and spray. Was encouraged by the likes of John Greven, Mike Doolin, and Gerald Shepard. Even Charles Fox. I was never able to achieve a finish that looked as good or held up as well as a professional nitro or catalyzed urethane application. I don't know about Greven but I think the others abandoned waterbased.

Has anyone here been selling guitars in the 3K plus range over a long period of time and finding customers satisfied with a waterbased finish?


My body chemistry destroys EM6000 on necks I switched to royal-lac for necks. All of the instruments I have sold with Em6000 on the necks held up well. I have had no problem on the body of the instrument and some I have had and played for seven or 8 years.

_________________
http://www.Harvestmoonguitars.com


Top
 Profile  
 
PostPosted: Tue Jan 16, 2018 1:14 pm 
Offline
Cocobolo
Cocobolo

Joined: Tue May 15, 2012 7:34 am
Posts: 137
First name: David
Last Name: Ingalls
City: Ashland
State: OR
Zip/Postal Code: 97520
Country: USA
Focus: Build
Status: Semi-pro
Here's Jay Lichty's video on EM6000:

https://www.youtube.com/watch?v=FXr9jYoikcA&t=621s


Top
 Profile  
 
PostPosted: Wed Jan 17, 2018 8:12 am 
Offline
Cocobolo
Cocobolo
User avatar

Joined: Sat Feb 02, 2008 9:19 am
Posts: 184
Focus: Build
Status: Amateur
Question for those still using EM6000. What have you found the useable shelf life to be of the finish? I used to use it but back then it was said most waterborne finishes had a one year shelf life, from the manufacture date. With this being the case I found it to be a very expensive finish for someone only finishing a couple guitars a year. Have any of you used it more than a year out? I know with lacquer the stated shelf life might be a year but I have had no problems after a much longer time.


Top
 Profile  
 
PostPosted: Wed Jan 17, 2018 12:22 pm 
Offline
Koa
Koa

Joined: Mon Oct 17, 2011 4:10 pm
Posts: 723
First name: Bob
Last Name: Gramann
City: Fredericksburg
State: VA
Zip/Postal Code: 22408
Country: USA
Focus: Build
Status: Professional
I’ve been using em6000 and its precursers for quite a while. I but it by the gallon and pour it into quart mason jars for storage and use. Sometimes, it takes me a couple of years to get to the bottom of the last quart. I’ve had no problems with it. I stopped having problems with neck finish dissolving from sweat when Target went from USL to em6000. The em6000 will dissolve under alcohol.


Top
 Profile  
 
Display posts from previous:  Sort by  
Post new topic Reply to topic  [ 19 posts ] 

All times are UTC - 5 hours


Who is online

Users browsing this forum: Colin North and 21 guests


You cannot post new topics in this forum
You cannot reply to topics in this forum
You cannot edit your posts in this forum
You cannot delete your posts in this forum
You cannot post attachments in this forum

Jump to:  
Powered by phpBB® Forum Software © phpBB Group
phpBB customization services by 2by2host.com