Status: Semi-pro
Thinking to use epoxy for gluing next fingerboard - I have araldite standard (high strength slow cure), have ordered Devcon 2 Ton Epoxy, and can also get BSI here in UK
Never thought to ask here what others recommend - duh

_________________
The name catgut is confusing. There are two explanations for the mix up.

Catgut is an abbreviation of the word cattle gut. Gut strings are made from sheep or goat intestines, in the past even from horse, mule or donkey intestines.

Otherwise it could be from the word kitgut or kitstring. Kit meant fiddle, not kitten.


Last edited by Colin North on Sun Jul 07, 2019 1:15 pm, edited 1 time in total.

Top
 Profile  
 
PostPosted: Sun Jul 07, 2019 12:53 pm 
Offline
Brazilian Rosewood
Brazilian Rosewood

Joined: Fri Aug 19, 2005 4:02 am
Posts: 3263
Location: The Woodlands, Texas
First name: Barry
Last Name: Daniels
I use West Systems. Whatever you use do the slow set kind. It usually cures harder than the quick set.


Top
 Profile  
 
PostPosted: Sun Jul 07, 2019 1:09 pm 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Wed Aug 12, 2009 1:13 am
Posts: 448
First name: Tim
Last Name: Allen
City: San Francisco
Focus: Build
Status: Amateur
I also use West System slow set, and it works well for me. I mix it by weight: I think the proportion is 3.7 to 1 part hardener. A small digital scale, cheap from eBay (about $15 US), makes it easy to mix even small amounts of epoxy accurately.

_________________
Tim Allen
"Never hurry, never rest."


Top
 Profile  
 
PostPosted: Sun Jul 07, 2019 1:40 pm 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Tue Aug 17, 2010 3:31 pm
Posts: 1682
First name: Kevin
Last Name: Looker
City: Worthington
State: OH
Zip/Postal Code: 43085
Country: USA
Focus: Build
Status: Amateur
Here's an old thread.

viewtopic.php?f=10101&t=39574&hilit=epoxy

_________________
I'm not a luthier.
I'm just a guy who builds guitars in his basement.
It's better than playing golf.



These users thanked the author klooker for the post: Colin North (Sun Jul 07, 2019 2:44 pm)
Top
 Profile  
 
PostPosted: Sun Jul 07, 2019 3:24 pm 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Wed Feb 15, 2006 7:37 am
Posts: 4805
I used Smith’s from LMI on my last, but this looks like one more reason to invest in some West.


Sent from my iPhone using Tapatalk



These users thanked the author James Orr for the post: Colin North (Sun Jul 07, 2019 3:58 pm)
Top
 Profile  
 
PostPosted: Sun Jul 07, 2019 3:54 pm 
Offline
Contributing Member
Contributing Member
User avatar

Joined: Fri Jul 10, 2009 4:44 am
Posts: 5498
First name: colin
Last Name: north
Country: Scotland.
Focus: Build
Status: Semi-pro
After some research and the replies to this post and others in the archives I think I'm leaning towards the Smiths https://www.makewoodgood.com/product/oak-teak-glue-wood-glue/

_________________
The name catgut is confusing. There are two explanations for the mix up.

Catgut is an abbreviation of the word cattle gut. Gut strings are made from sheep or goat intestines, in the past even from horse, mule or donkey intestines.

Otherwise it could be from the word kitgut or kitstring. Kit meant fiddle, not kitten.


Top
 Profile  
 
PostPosted: Sun Jul 07, 2019 5:19 pm 
Offline
Koa
Koa

Joined: Sun Oct 28, 2018 3:40 pm
Posts: 500
First name: Ernest
Last Name: Kleinman
City: Guthrie
State: OK
Zip/Postal Code: 73044
Country: United States
Focus: Build
Status: Professional
Contrarian here, I/ve used it and have 3 different types and 2 part UF glue . Frankly dont like it, for these reasons , Dont like the smell , , very messy application, and trying to remove it is, hard and cleanup is messy.. Once put on coco fb with epoxy , because of the oils and then had to remove it . Total pita. Your mileage and results will vary. I/ve had better luck using epoxy with a brush or roller for laminated sides . For FB . I prefer fish . long open time , . easy cleanup with warm water , easy to remove fb for repairs. I also use fish for frets , not ca,



These users thanked the author Ernie Kleinman for the post: CarlD (Sun Jul 07, 2019 8:08 pm)
Top
 Profile  
 
Display posts from previous:  Sort by  
Post new topic Reply to topic  [ 7 posts ] 

All times are UTC - 5 hours


Who is online

Users browsing this forum: No registered users and 50 guests


You cannot post new topics in this forum
You cannot reply to topics in this forum
You cannot edit your posts in this forum
You cannot delete your posts in this forum
You cannot post attachments in this forum

Jump to:  
Powered by phpBB® Forum Software © phpBB Group
phpBB customization services by 2by2host.com